Hello, Alphacool team!
About a year of operation on pure distilled water, black flakes began to appear in the circuit, the flow has dramatically decreased (microchannels of the water blocks are clogged). Inside, on surfaces in contact with water, bulges (bubbles) of the black coating have formed, it cleared with a regular plastic card effortlessly. The outer coating remains flawless, look perfect, but I know it all would be better with the usual nickel plating.
Cheers.
About a year of operation on pure distilled water, black flakes began to appear in the circuit, the flow has dramatically decreased (microchannels of the water blocks are clogged). Inside, on surfaces in contact with water, bulges (bubbles) of the black coating have formed, it cleared with a regular plastic card effortlessly. The outer coating remains flawless, look perfect, but I know it all would be better with the usual nickel plating.